Factors Affecting The Straight Seam High Frequency Welded Steel Pipe
Mar 08, 2024
- Welding frequency
The HF frequency affects the uniformity of current distribution within the steel plate. When selecting the high frequency welding frequency, both the depth of heat penetration and the proximity effect should be considered. Generally, the current frequency can be increased appropriately, not only to save power but also to improve the quality of the weld and reduce the size of the weld heat-affected zone. From the welding efficiency, as far as possible, the use of higher frequency. 100kHz high-frequency current can penetrate the ferritic steel 0.1mm, 400kHz can only penetrate 0.04mm, that is, the current density distribution on the surface of the steel plate, the latter than the former to be higher than nearly 2.5 times.
In production practice, welding carbon steel materials can generally be selected 350 ~ 450kHz frequency; welding alloy steel materials, more than 10mm plate thickness, can be used 50 ~ 150kHz frequency, because the alloy steel contains chromium, zinc, copper, aluminium and other elements of the skin effect with the steel has a certain difference.

- Welding V-angle
The size of the V-angle has a direct impact on the welding quality, V-angle when the neighbourhood effect is significant, is conducive to improving welding speed, but the preheating section and the melting section becomes longer, making the flash process is not stable, over the beam burst is easy to form a deep crater and pinhole, it is difficult to press together. V-angle is too large, the melting section becomes shorter, the flash is stable, but the neighbourhood effect is weakened, the welding efficiency is significantly reduced, and the power consumption increases. At the same time in the moulding of thin-walled steel pipe, V-angle is too large to make the edge of the pipe elongated, resulting in wavy wrinkles. V-angle in actual production is generally adjusted in 2 ° ~ 6 °, thin-walled pipe generally use a smaller convergence angle; thick-walled pipe welding speed is slower, extrusion moulding to use a larger convergence angle.

- Welding power
Power is too small billet bevel heating is not enough to reach the welding temperature, resulting in false welding, de-welding, welding and other welding defects; power is too large, it affects the welding stability, billet bevel surface heating temperature is much higher than the welding temperature, resulting in serious spatter, pinhole, slag and other defects, this defect is called the overcooking defects. High-frequency welding input power should be adjusted according to the thickness of the pipe wall and forming speed to determine the different forming methods, different unit equipment, different material steel grade, all need to be optimised through the practice summary.
Above are the factors affecting the quality of LSAW pipe for you, GNEE Group is a professional steel supplier, you can contact us at any time for your steel needs.