The most basic alloying elements of austenitic stainless steel are chromium and nickel. The representative grade is chromium-nickel austenitic stainless steel with a chromium content of about 18% and a nickel content of about 8%. The element ratio of chromium and nickel basically ensures that the structure of the steel is stable austenite. Austenitic stainless steel has developed rapidly. In order to meet the needs of different conditions, other alloying elements are added on the basis of 18-8 steel, giving this type of stainless steel better performance. The organizational structure of austenitic stainless steel determines that its mechanical properties are characterized by low strength and high plasticity and toughness. In my country's stainless steel standards, the given tensile strength of austenitic stainless steel is generally 480~520N/mm2, and some are 400N/mm2. According to the standard, no impact test values ​​are given for austenitic stainless steel forgings and rolled products. In fact, the impact energy of austenitic stainless steel after solution heat treatment can reach 120J or higher. The mechanical properties of austenitic stainless steel cannot be adjusted by heat treatment. 18-8 type austenitic stainless steel is corrosion-resistant to oxidizing media such as air, dilute nitric acid or medium concentration nitric acid and concentrated sulfuric acid. It has good corrosion resistance in sodium hydroxide and potassium hydroxide solutions within a fairly wide range of concentrations and temperatures. However, it is not corrosion-resistant in reducing media such as hydrochloric acid and sulfurous acid, nor in concentrated nitric acid. In addition, when austenitic stainless steel is slowly cooled in the range of 850 ~400°C after heating, chromium carbides will precipitate from the grain boundaries, causing local chromium-poor areas at the grain boundaries, thereby causing intergranular corrosion. The intergranular corrosion resistance of austenitic stainless steel is related to the carbon content. The lower the carbon content, the stronger the intergranular corrosion resistance. Austenitic stainless steel is sensitive to stress corrosion cracking. The nickel content in steel plays an important role in improving stress corrosion cracking resistance. According to the chemical composition and the purpose of heat treatment, the heat treatment methods commonly used for austenitic stainless steel include solution treatment, stabilization annealing treatment, stress relief treatment and sensitization treatment.

stainless steel pipe
(1) Solution heat treatment

The solution treatment of austenitic stainless steel is a process method in which the steel is heated to a certain temperature at which the excess phase is fully dissolved into the solid solution, and then rapidly cooled after being kept for a certain period of time. The purpose of the solution heat treatment of austenitic stainless steel is to dissolve the alloy carbides produced or precipitated in the previous processing steps, such as (FeCr) 23C6, etc. and o phase into the austenite, and obtain a single austenite structure (some may contain a small amount of 8 ferrite) to ensure that the material has good mechanical properties and corrosion resistance, and fully eliminate stress and cold work hardening. Solution treatment is suitable for austenitic stainless steel of any composition and grade. Solution treatment can greatly improve the corrosion resistance of stainless steel, eliminate work hardening, reduce hardness, etc. The main processing technology is to heat the steel to 1050~1150C, the holding time is calculated according to the material thickness or diameter (about 1h for every 25mm), and water quenching is mostly used for cooling.

(2) Stabilization heat treatment

Stabilization heat treatment is generally arranged after solution treatment and is commonly used for 18-8 steel containing tantalum and tantalum. The purpose of stabilization heat treatment of austenitic stainless steel containing tantalum and tantalum is to maximize the effectiveness of anti-intergranular corrosion. Since chromium carbide is completely dissolved, while tantalum carbide is not completely dissolved and fully precipitated during the cooling process, it is impossible for carbon to form chromium carbide, thus effectively eliminating the occurrence of intergranular corrosion. The main treatment process is generally arranged after solution treatment. The steel is heated to 850~950°C and fully insulated. The insulation time is based on the thickness or diameter (about 2h for every 25mm of insulation). After insulation, air cooling or furnace cooling is used. Steel grades without tantalum or tantalum cannot be stabilized, otherwise the effect will be counterproductive.

welded round pipe
(3) Stress relief heat treatment

The purpose of stress relief heat treatment of austenitic stainless steel is: Ⅰ. To improve the material's layer strength and fatigue strength without changing the material's plasticity. Ⅱ. Eliminate the stress corrosion tendency that may be caused by internal stress. The main treatment process is: For purpose Ⅰ, it can be heated at a lower temperature (300 ~ 350 ° C) for 1 ~ 2 hours and then air-cooled. For purpose Ⅱ, the heating temperature must be above 800 ° C and then quickly cooled after insulation. For steels containing tantalum or tantalum, slow cooling is used after insulation.
(4) Sensitization treatment

Sensitization treatment is actually not a heat treatment method that should be used in the production process of austenitic stainless steel or its products. Instead, it is a procedure used when testing the intergranular corrosion resistance of austenitic stainless steel. Sensitization treatment is essentially a treatment that makes austenitic stainless steel more sensitive to intergranular corrosion. For some special use occasions, in order to more strictly evaluate the material's intergranular corrosion resistance, in some standards, the sensitization system for austenitic stainless steel is more stringent, and different sensitization systems are used according to the future use temperature of the workpiece and the carbon content of the material and whether it contains tantalum elements. Some also control the heating and cooling speed of the sensitization treatment. Therefore, when determining the intergranular corrosion tendency of austenitic stainless steel, attention should be paid to the sensitization system used.

stainless steel round pipe

(5) Cold working strengthening and stress relief treatment of austenitic stainless steel

Austenitic stainless steel cannot be strengthened by heat treatment methods, but it can be strengthened by cold working deformation (cold hardening, deformation strengthening), which will increase strength and reduce plasticity. After cold working deformation strengthening, austenitic stainless steel or products (springs, bolts, etc.) have large processing stress. The existence of this stress increases the sensitivity of stress corrosion when used in a stress corrosion environment and affects the stability of dimensions. To reduce stress, stress relief treatment can be used. Generally, it is heated to 280~400°C and maintained for 2h~3h, then air cooled or slowly cooled. Stress relief treatment can not only reduce the stress of the product, but also improve the hardness strength and elastic limit without a significant change in elongation.

(6) Some issues that should be noted in the heat treatment of austenitic stainless steel.

First of all, attention should be paid to the reasonable selection of the heating temperature for the solution treatment of austenitic stainless steel. In the material standard of austenitic stainless steel, the specified solution heating temperature range is relatively wide. In actual heat treatment production, the specific composition, content, use environment, possible failure form and other factors of the steel can be considered to reasonably select the optimal heating temperature. However, care should be taken to prevent the melting heating temperature from being too high, because if the solution treatment heating temperature is too high, the grains of the material that has been refined by forging and rolling may grow. The coarsening of the grains will cause some adverse consequences. Secondly, attention should be paid to the effect of stabilization treatment on the performance of the solid solution state. For austenitic stainless steel containing stabilizing elements, when the solid solution heat treatment is followed by stabilization treatment, the mechanical properties tend to decrease. This phenomenon occurs in strength, plasticity and toughness. The reason for the decrease in strength may be that during the stabilization treatment, the strong carbide-forming element boron combines with more carbon to form TiC, which reduces the strengthening degree of carbon in the austenite solid solution. In addition, TiC will also grow in the heating and insulation process, which will also affect the strength.
Third, the heating temperature for stabilization treatment should not be too high, and is generally selected between 850~930°C. Austenitic stainless steel should not be subjected to multiple solid solution treatments, because multiple solid solution heating will cause grain growth and adversely affect the performance of the material. At the same time, attention should be paid to pollution during the processing, and once contaminated, measures should be taken to eliminate the pollution.