ASME SA 213 Grade T12 Alloy Steel Seamless Tubes
Oct 13, 2023
ASME SA 213 Grade T12 Alloy Steel Seamless Tubes
SA213 T12 Tube Specification
| Standard | ASTM A213 T12, SA213 T12 (with IBR Test Certificate) |
| Specifications | ASTM A213 & ASTM A209 (T1 , Ta, T1b) BS/3059/90/PartII/620 & 622 DIN/17175/13CrMo44 DIN/17175/10CrMo910 DIN/17175/15Mo3 |
| Size | 6.35 mm OD to 101.6 mm OD |
| Sch. & Swg. | 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg., 3.6 mm Thk |
| Thickness | 3-12mm |
| Origin | European, Japanese, Korean, US, Indian (Strictly No Chinese Material) |
| Tolerance | Cold drawn pipe: +/-0.1mm
Cold rolled pipe: +/-0.05mm |
| Craft | Cold rolled and Cold drawn |
| Type | Seamless / ERW / Welded / Fabricated |
| available in Form of | Round, Square, Rectangular, Hydraulic Etc. |
| Length | Standard Double & In Cut length also. |
| End | Plain End, Beveled End, Treaded |
| Specialized in | ASME SA213 T12 Boiler Tube, SA213 T12 Heater Tube, SA213 T12 Heat Exchanger Tube |
| SA213 gr T12 Additional Testing | NACE MR 0175, NACE TM0177, NACE TM0284, HIC TEST, SSC TEST, H2 SERVICE, IBR, etc. |
| SA213 grade T12 Tube Application | Seamless Ferritic Alloy Steel Tube for High-Temperature Service |

ASME SA 213 Grade T12 Properties
Chemical Properties
| Carbon | Silicon | Manganese | Phosphorous | Sulphur | Molybdenum | Nickel | Chromium | Copper | Others |
|---|---|---|---|---|---|---|---|---|---|
| 0.05-0.15 | 0.50 max | 0.30-0.61 | 0.025 | 0.025 | 0.44-0.65 | – | 0.80-1.25 | – | – |
Mechanical Properties
| Yield Strength | Tensile Strength | Elongation A5 min | |||
|---|---|---|---|---|---|
| MPa min | ksi min | MPa min | MPa min | ksi min | Percentage |
| 415 | – | 60 | 30 | ||