ASTM A213 T11 Alloy Steel Seamless Tube

Dec 05, 2025

ASTM A213 T11 Seamless alloy tubes description

T11 Alloy Tubes‌ are specialized high-alloy steel pipes classified as ‌martensitic heat-resistant steel‌, primarily used in high-temperature/pressure environments like heat exchangers and boiler piping.

‌Chemical Composition‌ includes carbon (C), silicon (Si), manganese (Mn), phosphorus (P), sulfur (S), and alloying elements such as chromium (Cr), molybdenum (Mo), and vanadium (V). Elevated Cr/Mo content enhances corrosion resistance, high-temperature stability, and mechanical properties, while V improves toughness.

‌Mechanical Properties‌:

High strength/hardness with good toughness

Post-heat treatment values:

Tensile strength: ‌≥450 MPa‌
-Yield strength: ‌≥300 MPa‌
-Hardness: ‌≥200 HB‌

Excellent fatigue and corrosion resistance

‌Heat Treatment Process‌:

‌Quenching‌: ~900°C (hold 2h) → air cooling

‌Tempering‌: ~650°C (hold 2h) → air cooling
Resulting microstructure: ‌Tempered martensite‌ delivering balanced mechanical properties.

 

ASTM A213 T11 Chemical Composition:

Chemical Components (%)
Grade C Mn P S Si Cr Mo
T11 0.05-0.15 0.30-0.60 ≤0.025 ≤0.035 0.50-1.00 1.00-1.50 0.44-0.65

 

Heat Treatment Requirements

Grade UNS Number Heat Treat Type Subcritical Annealing or Tempering Temperature, Min or range °F [°C]
T11 K11597 full or isothermal anneal normalize and temper 1200 [650]

 

ASTM A213 T11 Seamless alloy tubes Tensile Requirements and Hardness:

Mechanical Properties
Grade Tensile Yield Elongation Hardness
Strength (Mpa) Strength (Mpa) (%) (HRB)
T11 ≥415 ≥220 ≥30 ≤85

 

Mechanical Testing & Grain Size Requirements‌

‌Tensile Test‌

For lots of ‌less than 50 tubes‌: One test from a single specimen.

For lots of ‌over 50 tubes‌: One test each from specimens of two tubes.

‌Flattening Test‌

One test at ‌each end‌ of one finished tube per lot, ‌other than the tube used for flaring test‌.

‌Flaring Test‌

One test at ‌each end‌ of one finished tube per lot, ‌other than the tube used for flattening test‌.

‌Hardness Test‌

‌Brinell or Rockwell hardness test‌ on specimens from two tubes per lot.

‌Grain Size‌

Grain size determination shall be conducted on ‌one end of one finished tube‌ per lot to verify compliance with specified requirements.

test

 

Packaging and shipping

shipping