Low-alloy heat-resistant steel welding process points

Mar 13, 2024

  • Preparation before welding

For general low alloy heat-resistant steel weldments, various hot cutting methods can be used to undercut. In order to prevent cracking of the hot cutting edge of the thick plate, you can use the edge preheating, machining and magnetic particle detection of the presence of surface cracks. Hot cutting edges or bevelled surfaces such as direct welding, welding must be cleaned before hot cutting slag and oxide skin. Cutting surface notch should be grinding wheel grinding smooth transition, machined edges or bevelled surfaces should be removed before welding oil and other dirt. For weldments with high quality requirements, it is best to wipe the bevelled surface with acetone before welding.

Welding materials should be properly pre-treated before use. Light wire surface rust oil should be removed, welding rod or flux in addition to proper storage, before use, should be strictly in accordance with the provisions of the procedure for drying, which is important to maintain the low hydrogen content of the weld metal.

A335 P91 alloy steel pipe

  • preheating, post-heating and post-weld heat treatment

Preheating is one of the effective measures to prevent cold cracking and reheating cracking of such steel welded joints. Preheating temperature is mainly based on the carbon content of steel, joint constraints and hydrogen content of the weld metal to determine the preheating temperature of low-alloy heat-resistant steel and the interlayer temperature shall be lower than the temperature of the end of the martensitic transformation point, the end of the welding, austenite immediately in the temperature of the interlayer transformed into martensite, and in the complete end of the martensitic transformation and then post-weld heat treatment, so that the martensite organisation is tempered to form a higher toughness Tempered martensite. The key to this welding process should be the end of welding to post-weld heat treatment interval included in the process control range. In welding small weldments, such as the use of electric heaters preheating and post-weld heat treatment is possible. But for large weldments, such as the use of flame preheating weldments and welded into the furnace heat treatment, from the end of welding to the furnace during this period of time, the joints produce a greater risk of cracking. In order to prevent the weldment from cracking before the post-welding heat treatment, the welded joints need to do post-heat treatment. Post-heat treatment according to the type of steel and wall thickness, generally 200 ~ 350 ℃, time greater than 0.5h, in order to prevent hydrogen cracking.

Local preheating of large weldments should be careful to ensure that the width of the preheating zone is greater than 4 times the welded wall thickness, at least not less than 150mm, and the preheating zone should reach the specified temperature on both the inner and outer surfaces. In the welding process, the preheating temperature should be kept basically the same, which is often the key to success or failure of welding.

A335 P22 alloy steel pipe

  • the choice of welding heat specification

Welding heat specification usually refers to the welding heat input, preheating temperature and interlayer temperature. Welding heat specification directly affects the cooling conditions of the joint. The larger the heat specification, the slower the cooling rate, the joints of the region of the grain is more coarse, the lower the strength and toughness. The use of low heat specification, you can improve the cooling rate of the joints, is conducive to the refinement of the joints of the grain, improve the microstructure and improve the impact toughness, but in the low-alloy heat-resistant steel welding, preheating and maintaining the interlayer temperature is to prevent the joints of one of the conditions of cold cracking, so the adjustment of the welding heat specification is mainly through the control of the weld heat input. Most low-alloy heat-resistant steel is not sensitive to changes in welding heat input within a certain range. In order to prevent cold cracking, it is hoped that the welding heat input is not too small. Only when the welding heat input exceeds 30kJ/cm, preheating and interlayer temperature exceeds 250 ℃, Cr-Mo steel weld metal strength and impact toughness will be significantly reduced.

  • the impact of post-weld heat treatment

Cr-Mo heat-resistant steel post-weld heat treatment specifications for its strength, especially toughness has a significant impact, usually with the value of tempering parameters to evaluate the degree of its impact, the value of tempering parameters by the heat treatment of the temperature and holding time decision. For each kind of Cr-Mo heat-resistant steel has an optimal range of tempering parameters, and therefore also corresponds to an optimal post-weld heat treatment temperature and time.