Reasons why the hardness value exceeds the standard during alloy steel pipe welding

Mar 05, 2024

1. Improper temperature control

The welding temperature needs to be controlled during welding. If it is too high or too low, the hardness value will exceed the standard. If the welding temperature is too high, the structure in the weld will be coarsened and the hardness will increase; if the welding temperature is too low, the weld will be cold cracked. For carbon steel and low alloy steel, the general welding temperature is between 600°C and 700°C.

alloy steel welded pipe

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

2. Material mismatch

Material mismatch is also one of the reasons why the hardness value of the weld exceeds the standard. When selecting welding materials, the composition differences between the steel pipe and the welding materials should be taken into consideration, otherwise the hardness of the weld will be too high. For low alloy steel, you can use appropriate alloy welding materials such as molybdenum, chromium, titanium and other elements to improve the toughness of the weld and avoid excessive hardness values.

welded alloy steel pipe

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

3. Welding speed is too fast

Excessive welding speed will also cause the hardness value of the weld to exceed the standard. In the case of rapid cooling, the structure will harden, resulting in an increase in the hardness value of the weld. The welding speed should be controlled so that it is not too fast and not too slow to avoid excessively high hardness values.