1. Tube blank heating
Heating should be evened to prevent rapid rise and fall in temperature. Each rising and falling temperature should be stable and slow, and the rising and falling temperature should not exceed 30°C.
2.Rolling mill mandrel
Thick-walled tubes with average wall thickness and solid blanks greatly reduce the possibility of bending deformation of the mandrel and can effectively improve the wall thickness accuracy of steel pipes.
3. Precision of mandrel
The external processing accuracy of the mandrel is controlled within ±0.1mm, and the straightness deviation of the mandrel does not exceed 5mm. During the welding process, precision machined pins are inserted between the two mandrels for positioning to prevent the overall straightness of the weld from being too large.,

lsaw carbon pipe
4.Process
Determine whether the centering roller device is in place, adjust the center of the relevant core clamping roller, the opening angle of each action and the size of the opening teeth, and the center of the core clamping roller must be on the rolling line
5. Centering roller
Technically, in order to avoid the occurrence of center thinning and wall thickness increase, as well as the situation where the thickness exceeds the control range, the wall thickness accuracy is improved.
6.Perforator
The ejector rod with a hole usually chooses a thick-walled tube with an outer diameter of Φ108mm-Φ114mm, a wall thickness of ≥25mm, and an average wall thickness.
7. Rolling center line
Make sure that the rolling center line of the piercing machine is consistent with the center line of the piercing car to prevent "rolling up" or "rolling down" so that the tube blank maintains uniform force during the piercing process.

saw welded pipe
8. Rolling things
Worn plugs, guide plates, rollers and other rolling items should be replaced in time.
9. Rewinding device
The middle of the roll pitch and the guide pitch must be on the rolling line. Make sure that the center line between the guide spacing and the rolling spacing is on the middle line of the perforation and rolling, that is, the upper and lower rolling spacing are equal, and the left and right guide spacing are equal.