A335 P5 Alloy Tube: 5Cr-0.5Mo Seamless Pipe for Refinery and Boiler Service

Feb 27, 2024

A335 P5 Alloy Tube Overview

ASTM A335 P5 is a 5Cr-0.5Mo ferritic alloy-steel tube grade for high-temperature service. The chromium content gives it useful resistance to high-temperature oxidation and to the sulfur-bearing streams found in refining, while the molybdenum addition raises creep strength well above that of carbon steel. The same chemistry appears as T5 when the product is ordered as tubing to ASTM A213, and the two designations share the same allowable stress data.

A335 P5 tube is normally supplied seamless, hot finished or cold drawn depending on size, in the annealed, normalised and tempered, or stress-relieved condition.

Chemical Composition and Mechanical Properties

Element Typical range, %
C 0.15 max
Mn 0.30 – 0.60
P 0.025 max
S 0.025 max
Si 0.50 max
Cr 4.00 – 6.00
Mo 0.45 – 0.65

Minimum tensile strength: 415 MPa

Minimum yield strength at 0.2% offset: 205 MPa

Minimum elongation in 50 mm: 30%

Hardness and grain size limits: as specified by ASTM A335 / A335M

General requirements, tolerances and testing: ASTM A450 / A450M

Petrochemical and Refining Applications

Process plants use A335 P5 where temperatures are too high for carbon steel but the duty does not justify an austenitic or higher-chromium grade. Typical duties include:

Transfer, charge and recycle lines in refining and petrochemical units

Heater and furnace outlet piping and cracking coil supports and hangers

Hydrogen-bearing process lines and high-pressure hydrogen equipment parts

Heat exchanger tubes, valve bodies, pump parts and piston rods

Fasteners and steam turbine cylinder linings exposed to hot steam

The grade resists high-temperature sulfidation better than carbon and low-chromium steels, which is why it appears in streams that carry sulfur compounds at elevated temperature. It is not intended for strongly oxidising acid service, where a stainless grade is required.

Power Generation and Boiler Tubing

In power plants the tube is used for superheater and reheater elements, main and reheat steam piping, boiler hangers and headers where metal temperature stays within the creep range of 5Cr-0.5Mo steel. Because the allowable stress of P5 falls as temperature rises, wall thickness must be calculated from the design metal temperature and the hot allowable stress table, not from the room-temperature tensile value.

Design basis: allowable stress at design temperature per the applicable piping or boiler code

Corrosion allowance additional to the calculated pressure wall

Thermal expansion taken into account in the support and hanger layout

Bends and fittings specified in the matching P5 chemistry

Fabrication, Welding and Inspection Notes

5Cr-0.5Mo steel hardens when it cools quickly, so both fabrication and welding follow a controlled thermal route.

Preheat before welding, typically 150 – 200 °C, with interpass temperature kept in a narrow band.

Filler metal of the matching 5Cr-0.5Mo class, such as a B6 type electrode or wire, rather than carbon steel filler.

Post-weld heat treatment after welding to relieve stress and restore toughness in the weld and heat affected zone.

Tubes bent cold are stress relieved afterwards where the code or the specification requires it.

Inspection covers dimensional control of outside diameter and wall, visual and non-destructive examination of the body and ends, and a hydrostatic or eddy current test as ordered. Each lot is supplied with a mill test certificate giving ladle analysis, tensile results and the heat treatment condition.

Frequently Asked Questions

Q: What does the P5 designation actually mean?
It identifies a 5 percent chromium, 0.5 percent molybdenum ferritic alloy steel in the ASTM A335 / A335M pipe specification. The P prefix is used for pipe, the T prefix for the same chemistry supplied as tubing to ASTM A213.

Q: What is the maximum service temperature for A335 P5 tube?
It is used in the creep range and its allowable stress decreases as temperature rises. The limit for a given line is set by the allowable stress at design temperature in the governing code rather than by a single fixed number.

Q: Can A335 P5 be welded to carbon steel?
Yes, with a qualified dissimilar joint procedure using a suitable nickel-bearing or matching alloy filler. The joint still requires controlled preheat and a post-weld heat treatment, and the procedure must cover the actual thicknesses involved.

Q: Why is post-weld heat treatment required?
Welding creates a hard, stressed heat affected zone. Heat treatment in the tempering range reduces residual stress, softens the zone to an acceptable hardness and restores toughness so the joint can survive thermal cycling in service.

Q: How should the tube be stored before installation?
It should be kept dry, supported along its length and protected at the ends. Carbon and alloy tubes are stored separately to avoid contact corrosion, and the heat number marking is preserved so the tube can be matched to its certificate.