A213 T22 and A213 T92 are two different alloy steel tubes that differ in chemical composition, strength and application:
Chemical composition:
A213 T22: Contains 2.25% chromium and 1% molybdenum, which are its main alloying elements and contribute to the steel's high temperature strength and corrosion resistance.
A213 T92: Contains 9% chromium and 0.9% molybdenum with the addition of vanadium, nitrogen and tungsten, these additions improve the steel's resistance to high temperatures and enable it to maintain its strength at higher temperatures.

Mechanical properties:
A213 T22: This steel has a tensile strength of 415 MPa, a yield strength of 205 MPa, an elongation of 30% and a hardness of less than or equal to 163 HBW.
A213 T92: It has higher tensile strength (≥620MPa) and yield strength (≥440MPa), which indicates that it has better performance in high temperature and high pressure environments.

Applications:
A213 T22: It is commonly used in petrochemical and power industries, especially in the manufacture of high temperature and high pressure pipes, heat exchangers and reactors.
A213 T92: Due to its excellent high-temperature performance and durability, it is commonly used in power station boilers and the nuclear power industry, especially in scenarios requiring higher temperature and pressure resistance.
To summarise, A213 T92 outperforms A213 T22 in scenarios where high temperature performance and application requirements are more stringent, while A213 T22 is better in terms of economy and moderate high temperature performance.